Harmony Hard is a high gold casting alloy with a distinct yellow colour. Due to the good processing properties and the wide range of indications when heat-treated, this alloy can be used for many different applications.
Composition (%): | Au 74.0 | Pd 3.8 | Ag 12.0 | Cu 9.0 | In <1.0, Ir <1.0, Zn <1.0 |
ISO | 22674:2016 |
ADA Class | High Noble |
Type / Color | 2 / Yellow |
Density (g/cm³) | 14.9 |
Melting Range (Solidus/Liquidus): | 895 - 970 °C |
Elastic Modulus (GPa): | 86 |
As Cast Softened Hardened | |
Vickers Hardness: | 130 130 180 |
Tensile Strength (MPa): | 430 395 475 |
0.2% Proof Stress (MPa): | 260 255 330 |
Elongation (%): | 40 45 30 |