demo title

d.SIGN 30

Co-Cr (60.2% & 30.1%)-based dental metal-ceramic alloy, Type 5

Advantages

  • Light oxide
  • Tested biocompatibility

Processing Data

Investment Material:  Phosphate-bonded
Preheating / Burn- out Temperature: 800 - 850 °C
Crucible  Ceramic crucible
Casting Temperature: 1240 - 1300 °C
Oxidation  °C/min/Vacuum: 925 / 5 / Yes
CTE: (25 – 500 °C): 14.5 x 10-6 /K
Laser Welding Wire: Laser Ceramic White

*See TYPE CLASSIFICATION DUE TO PHYSICAL PROPERTIES